Nanoindentation in alumina coated Al: Molecular dynamics simulations and experiments
| Categories |
Zeitschriftenbeiträge, begutachtet |
| Year | 2022 |
| Authors | Luu, H.-T., Raumel, S., Dencker, F., Wurz, M., Merkert, N. |
| Published in | Surface and Coatings Technology 437, p. 128342 |
Description
Nanoindentation in alumina coated Al: Molecular dynamics simulations and experiments
| DOI | 10.1016/j.surfcoat.2022.128342 |